Temperature at which moisture will condense on surface. No coatings should be applied unless surface temperature is a minimum of 5° above this point.Temperature must be maintained during dry through.
Example:
If air temperature is 60°F and relative humidity is 50% the dew point is 40°F.No coating should be applied unless surface temperature is 45° minimum.